Would it be possible to powder coat this part? Its plastic but it seems heavy duty. How hot does the PC process heat up the parts?
[/color][/b][/i][/size]
About 400-degrees F...the "plastic" is actually a type of Bakelite phenolic resin & it will be destroyed by that type of heat. Hammertone Silver looks fantastic on the bottle door anyway, don't over engineer the process. also beware it is somewhat prone to brittle with age, so don't pry on it or drill into it to aggressively. it WILL crack or shatter. and easy on the drilling pressure as the aft end of the drilled hole will try to blow out when the bit drills through the door. treat it like working with glass...